Fig 2Laying the transfer filmHold to brake · SpaceStop 0 · film 0.0 μm · μ 0.49 · peak —
Transfer film on the friction ring: 1–3 μm, renewed as the pad brakesPad on the loading arm; the slotted weights set the clamp forceGauges: drag dial (μ), micron dial on a slide (film), thermocouple meter (°C)Each stop lays a little more pad material on the disc until an even transfer film of 1–3 μm has formed; with it, μ holds at 0.55–0.57 from 100 to 800 °C instead of climbing from 0.49, and the peak temperature falls from 828 to 690 °C (Barbaro RS-652 dyno data, steel disc). The stop-by-stop build-up is schematic; holding the clamped pad on a hot, stopped disc prints an uneven patch that the next stops wear back down.