The science
of stopping.
Every compound engineered from first principles — friction, thermal stability and wear balanced at the molecular level.
Curves, not flat lines.
Friction coefficient across operating temperature. Select a compound to redraw its thermal behaviour.
A 1–3 micron transfer film, continuously self-renewing — the Barbaro signature.
Constant friction
The film renews as fast as it wears — the pad-rotor interface never changes character mid-stint.
Rotor protection
Disc attack is absorbed by the sacrificial film, not the rotor — 0.001 mm disc wear per cycle on RS-652.
Lower peak temps
Once stabilized, peak interface temperatures fall — −16.7% on steel, −12.8% on carbon-ceramic.
Eight compounds.
At a glance.
| Model | Formula type | Temp rating | Friction range | Standard / Eco |
|---|---|---|---|---|
| C-01 | Low-Metallic | 550°C | 0.40–0.48 μ | EU & US environmental standards |
| C-02 | Ceramic NAO | 550°C | 0.38–0.42 μ | Contains copper |
| C-60 | Adv. Low-Metallic | 600°C | 0.48–0.55 μ | EU & US environmental standards |
| S-01 | Semi-Metallic | 800°C | 0.35–0.50 μ | N/A (semi-metallic) |
| RS-620 | Race Low-Metallic | 50–800°C | 0.38–0.48 μ | N/A (race only) |
| RS-635 | Race Endurance | 50–800°C | 0.40–0.52 μ | N/A (race only) |
| RS-652 | Race Hybrid · Steel + CCB | 50–800°C | 0.49–0.57 μ · CCB rising | N/A (race only) |
| CSI-01B | Carbon-Ceramic Specific | −30–600°C | 0.40–0.43 μ | SAE J2521 noise rating AA |
Seven dimensions.
Street Series rated across seven critical dimensions; Race and Carbon-Ceramic Series validated through bench tests and on-track results.
Tested to
global standards.
| Model | Designated friction | Grade | SAE mean friction | SAE range | Temp range |
|---|---|---|---|---|---|
| RS-620 | 0.482 | GG | 0.45 | 0.45–0.85 | 50–800°C |
| RS-635 | 0.481 | GG | 0.47 | 0.45–0.90 | 50–800°C |
All compounds additionally validated against GB5763-2018 national standards.